  Q1.a) what do you mean by terminal solid solutions?                                                    (10 marks)
       b)Describe the destinctions between hypo eutectoid and hyper eutectoid steels?
      c)what is hardenabilition?
     d)briefly explain transmissive and reflective modes of operation for electron and opticalmicroscopes?             
    e)state Peritectic reaction with an example?
Q2.a) from the following alloys .pick the one that may be strengthened by heat treatment ,cold work or both 410 stainless steel, 4340steel, F10004castiron,C26000 cartridge brass,356.0 aluminum ,ZK60A magnesium ,R56400 titanium, 1100 aluminium, and zinc .explain reasons about your selection. (5 marks)
    b) copper has FCC structure and its atomic radius is 1.273 amstrongs.Find the lattice parameter and density of the copper (atomic weight copper =63.5 gm/mol.)    (5marks)
    c)why low carbon steels are not heat treatable and state how can their strength be increased?(5 marks)
                                                                                                                                                        PART-B
Q3.
a)what are point defects? Explain in detail the different types of point defects with suitable sketches?(15marks)
b)what are surface defects ? explain with suitable sketches the different types of surface defects.?
Q4.
a)sketch iron-iron  carbide phase diagram .explain about development of micro structure in iron carbon alloys by elaborating on important chemical reactions occurring during phase changes. (15 marks)
Q5.
Two metals A&B have melting point of 650 & 450 degree c respectively when alloyed together they did not form any compound or intermediate phase but form a eutectic at 300 degree c of composition of 40 percentage  .A the maximum solubilities of bin A& A in B occurring at 300 c are 10 % B & 8%A respectively and they reduce to 5 %B & 4% A respectively  at 0 degree c .assume the solidus,  liquidus  & solvus line to be straight
a)      Draw the phase diagram of the series and mark all salient regions.                                                                                                 (15 marks)
b)      Find the temperature at which an alloy with 30%B starts & ends solidification.
c)       Find the relative amounts , percentages, composition ,number ,type & distribution of the phases in the above alloy at 0 degree c .
Q6.
Explain in detail about the various microscopic examination / characterization techniques. Elaborate on optical microscopy, working principle, optical microscope construction, and applications in material science and engineering.                                                                               ( 15 marks)
                                                                                                                                                               PART-C  
Q7. Consider the hypothetical eutectic phase diagram given below and assume that (!); alpha and beta phases and exist at the   A & B extremities of the phase diagram.                    (15 marks)
(2) The eutectic composition of the alpha phases at the eutectic temperature is 88 wt%A-12wt%B.
Determine the composition of an alloy that will yield primary Beta and total Beta mass fraction of 0.367 and 0.768.respectively in iron iron carbide diagram.
Q8.
Provide an analytical  assessment whether it would be advisable to hot work or cold work the following metals/alloys on the basis of melting temperature ,oxidation resistance, yield strength and degree of brittleness:platinum,lead,molybdenum,304-stainless steel and copper . (15 marks)
Q9.
Consider the gas carburizing of a gear of steel at 920 degree c .calculate the time in minutes necessary to increase the carbon content to 0.4% at 0.5mm below the surface. assume that the carbon content at the surface is 0.9% and the steel has a nominal carbon content of 0.2%.(15 marks)